TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Date:
Thu, 10 Sep 2009 19:05:51 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, stephengregory5849 <[log in to unmask]>
Subject:
From:
stephengregory5849 <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<EC55942490AF4B3CACE4CC6526408635@ingemar63eaed8>
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=response
MIME-Version:
1.0
Parts/Attachments:
text/plain (261 lines)
Hi Inge,

A little late in the day, but I have your pics posted. They are here:

http://stevezeva.homestead.com/1.jpg
http://stevezeva.homestead.com/2.jpg
http://stevezeva.homestead.com/3.jpg
http://stevezeva.homestead.com/4.jpg
http://stevezeva.homestead.com/5.jpg

Yep, MK-46's were what we carried, at the tail-end we were starting to carry 
AGM-84 Harpoons which made us P-3's more of a target IMHO. Also, although 
it's not a concealed and carry, what makes me comfortable and gives me a 
warm and fuzzy is a Barrett Model 82A1. It's almost like a hand grenade, you 
only need to get close with that...heh

Steve


----- Original Message ----- 
From: "Inge" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, September 10, 2009 12:24 PM
Subject: Re: [TN] Need clever comments


>I will post a handful SEM images to Steve, so you get an idea what it's all 
>about.
> It may take a while, because he is probably on the market place to buy 
> curtains and  wallpaper
> for his new appartment. Or jogging. Or having a drink on the balcony.
> /Inge
>
>
> ----- Original Message ----- 
> From: "Inge" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Thursday, September 10, 2009 5:10 PM
> Subject: Re: [TN] Need clever comments
>
>
>> Jack &Paul, FYI.
>>
>> Today I had a close look at the cross sections. What I found was this:
>>
>> 1. The Tin plating was done AFTER solder mask (Jack was right)
>> 2. The solder mask was very uneven, thickness between 5um and 25 um.
>> 3. Despite the corrupted surface, the solder mask is homogenous, no 
>> vertical cracks found.
>> 4. The copper that I found earlier on top of the conductor, i.e. on the 
>> solder mask, that copper had no connection with the conductor copper. 
>> Which means that these contaminations had NOT migrated through the solder 
>> mask.
>> 5. I can still not figure out from where the copper contaminations come.
>>
>> So, all that remains is the question about the copper contaminations tha 
>> embedded in the very surface of the solder mask. I have to adjust my 
>> report and resend it to our customer and the board maker.
>>
>> Thanks to your critisism,  I can now redo the analys, starting from a 
>> more correct standpoint.
>>
>> Your are great!
>>
>> /Inge
>>
>>
>>
>>
>> ----- Original Message ----- 
>> From: "Inge" <[log in to unmask]>
>> To: <[log in to unmask]>
>> Sent: Wednesday, September 09, 2009 8:09 PM
>> Subject: Re: [TN] Need clever comments
>>
>>
>>> Jack,
>>>
>>> SMOBC is the common industrial standard, as you pointed out, however, 
>>> there ARE some fabricators that apply the solder mask after Tin/Lead-ing 
>>> the copper traces. The later method has an obvioius disadvantage, see 
>>> below quoted from an article written by US Environmental Agency:
>>>
>>>  " This method predominates for several reasons. Copper is a surface 
>>> that lends itself to rigorous cleaning, which is essential for solder 
>>> mask adhesion. Tin-lead under solder mask will liquefy during soldering 
>>> and may cause the mask to blister and peel. The hot air solder leveling 
>>> process generally produces less waste water and introduces less lead 
>>> into the waste water stream than tin-lead plating and reflow. Despite 
>>> these advantages, well-known disadvantages also exist. The shelf-life of 
>>> hot air solder leveled circuits is short and solder thicknesses on pads 
>>> and hole barrels is notoriously difficult to control. For these reasons, 
>>> a small minority of specifications continue to call for tin-lead plate 
>>> and reflow or other alternati air solder leveling, nomenclature 
>>> screening, and finally, gold edge plating if necessary. "
>>>
>>> I think that is what happened to our boards....." cause the mask to 
>>> blister and peel"...
>>>
>>> Another paper describes Tin under solder mask this way:
>>>
>>> " Facility F initially was concerned with the soldermask breakdown where 
>>> the Tin leaches underneath the soldermask....etc"
>>>
>>> Quoted from  EPA (United States Environmental Protection Agency.
>>>
>>> When I started the investigation (had just some hours to spend before 
>>> reporting the result!), I was fully convinced that these boards were 
>>> SMOBC, but our customer said they used tinning before soldermask. I have 
>>> asked for a confirmation from the board fabricator, but got no answer.
>>>
>>> Thanks for your comment, good critics.
>>>
>>> Inge
>>>
>>>
>>> ----- Original Message ----- 
>>> From: "Jack Olson" <[log in to unmask]>
>>> To: <[log in to unmask]>
>>> Sent: Wednesday, September 09, 2009 4:44 PM
>>> Subject: [TN] Need clever comments
>>>
>>>
>>>>I know I'm late to the game, but I can't resist asking this question:
>>>>
>>>>>From my experience, the tin is applied AFTER soldermask, so
>>>> you have mask over bare copper, and tin over exposed copper.
>>>>
>>>> The tin in PHOTO2.JPG in the exposed area looks beautiful,
>>>> so isn't the question (ignoring the whiskers for the moment)
>>>> "How can bare copper erupt through the mask?"
>>>>
>>>> Unless I missed one of your previous posts, it seems to me that
>>>> any speculation about copper poking through the tin finish is
>>>> irrelevant. I'm only addressing Question 2 below, but you mentioned
>>>> introducing a nickel barrier, and that will not be plated under the 
>>>> mask
>>>> either, will it? only on exposed circuitry...
>>>>
>>>> just wondering,
>>>> Jack
>>>>
>>>>
>>>> -=-=-=-
>>>>
>>>>  *Subject:* Need clever comments *From:* Hernefjord Ingemar <
>>>> [log in to unmask]> *Reply-To:* TechNet E-Mail Forum <
>>>> [log in to unmask]>, Hernefjord Ingemar <[log in to unmask]> 
>>>> *
>>>> Date:* Mon, 7 Sep 2009 13:21:54 +0200 *Content-Type:* text/plain
>>>>
>>>>
>>>> Hi all, need some professional backup regarding MIL quality boards.
>>>>
>>>> Objects: FR-4 Class III double-sided multi-layer boards, populated
>>>> with SOICS, BGAs,and a lot of passive components.
>>>>
>>>> Observation 1 : the non soldered board have lots of Tin whiskers on
>>>> inside of the PTH barrel. My thought is this: if whiskers can grow
>>>> long before the board is assembled, then ain't it likely that even CAF
>>>> can be generated?  See photo 1.
>>>>
>>>> Observation 2:  Copper has somehow penetrated the solder mask. This
>>>> can be found everywhere along the conductor traces. You need a very
>>>> good light microscope and a SEM to see it. See photo 2.
>>>>
>>>> Board data: Copper with 0.8 micrometer Immersion Tin. No nickel
>>>> barrier. Solder mask thickness not specified.
>>>>
>>>> Application: Typical MIL-883 environment
>>>>
>>>> Q1: What is your opinion about that thin Tin directly on copper? I
>>>> dislike the concept. Copper is very mobile at high temperatures, and
>>>> combined with humidity, there can be leakage currents and corrosion
>>>> issues. Even if the boards are CCd, there is a risk with copper .
>>>>
>>>> Q2: I gave  the advice to introduce a nickel barrier, but our customer
>>>> claimed, that they can't because of pressfit connectors and pressfit
>>>> test pins on the board. Furthermore, they had heard that one cannot
>>>> have nickel platings when pressfitting, because the nickel will crack
>>>> and oxidize and cause electrical disfunction. Is this your opinion
>>>> too? Are there any relevant testing behind such statements?
>>>>
>>>> Thanks in advance
>>>>
>>>> Inge
>>>>
>>>> ---------------------------------------------------
>>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>>> To unsubscribe, send a message to [log in to unmask] with following text 
>>>> in
>>>> the BODY (NOT the subject field): SIGNOFF Technet
>>>> To temporarily halt or (re-start) delivery of Technet send e-mail to 
>>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>>> To receive ONE mailing per day of all the posts: send e-mail to 
>>>> [log in to unmask]: SET Technet Digest
>>>> Search the archives of previous posts at: 
>>>> http://listserv.ipc.org/archives
>>>> Please visit IPC web site 
>>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
>>>> information, or contact Keach Sasamori at [log in to unmask] or 
>>>> 847-615-7100 ext.2815
>>>> ----------------------------------------------------- 
>>>
>>> ---------------------------------------------------
>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>> To unsubscribe, send a message to [log in to unmask] with following text 
>>> in
>>> the BODY (NOT the subject field): SIGNOFF Technet
>>> To temporarily halt or (re-start) delivery of Technet send e-mail to 
>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>> To receive ONE mailing per day of all the posts: send e-mail to 
>>> [log in to unmask]: SET Technet Digest
>>> Search the archives of previous posts at: 
>>> http://listserv.ipc.org/archives
>>> Please visit IPC web site 
>>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
>>> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
>>> ext.2815
>>> ----------------------------------------------------- 
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to 
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to 
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: 
>> http://listserv.ipc.org/archives
>> Please visit IPC web site 
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
>> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
>> ext.2815
>> ----------------------------------------------------- 
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> ----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------