TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wGspY-000Bk7C; Mon, 14 Apr 97 15:58 CDT
Encoding:
42 Text
Old-Return-Path:
Date:
Mon, 14 Apr 97 16:04:14 cst
Precedence:
list
Resent-From:
Cc:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11940
From [log in to unmask] Mon Apr 14 16:
04:40 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"DdE3o.0.pII.offKp"@ipc>
Subject:
From:
"ddhillma" <[log in to unmask]>
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
Message-Id:
Parts/Attachments:
text/plain (55 lines)
     Hi Ron -
     
     Take a look at JSTD-005 "Requirements for Soldering Pastes" - it has a 
     nice solder paste slump pattern that works well for many types of 
     slump variations. One additional check you may want to do - evaluate 
     your solder paste for slump AFTER component placement. Many solder 
     pastes do well in slump test in the as-printed configuration but fail 
     miserably after at component has been place on top of the print (for 
     20 mil pitch (and finer) components this is a big deal). Good Luck.
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: Subj:  Paste testing
Author:  [log in to unmask] at ccmgw1
Date:    4/14/97 3:13 PM


     
     Has anyone out there performed some hot and cold slump test?  Have you 
     run accelerated hot slump tests on paste?  If so at what temperatures?
     
     Is there a test plan for these tests?  If so, where can I find the 
     documents to follow the test plan?
     
     Thanks
     [log in to unmask]
     
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2