TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Wed, 16 Apr 1997 13:02:31 -0400 (EDT)
Precedence:
list
Resent-From:
From [log in to unmask] Wed Apr 16 13:
01:41 1997
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12033
X-Sender:
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"WS1Qx.0.KO8.2GGLp"@ipc>
Subject:
X-Priority:
1 (Highest)
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wHXxT-000BlyC; Wed, 16 Apr 97 11:53 CDT
From:
X-Mailer:
Windows Eudora Light Version 1.5.4 (16)
Message-Id:
Parts/Attachments:
text/plain (24 lines)
 We process the electro gold plating jobs (immersion type) in the following 
manner,

    RESIST STRIP->ALKALINE ETCH->TIN STRIP->PHOTO PRINT/DEVOLOP->GOLD PLATING


 This process is follwed by us,as we maximise the panel size due to which
the tabs are generally not to the edges. please suggest if any other process/
route is possible.

thanks..

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2