TECHNET Archives

March 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Douglas Pauls <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 17 Mar 2011 16:31:39 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (98 lines)
Thank you Inge,
Yes, Oneida first came to mind as they do an excellent job for Rockwell 
when we need RGA analysis, but they said the presence of liquid would foul 
their analysis.

Doug Pauls



Inge Hernefjord <[log in to unmask]> 
03/17/2011 04:23 PM

To
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
cc

Subject
Re: [TN] Hydrogen gas analysis






Hi Dough,
 
why does he ask? Of course it's >H2 or ions of H. There are numbers of 
sniffers, e.g. this one:
 
http://www.makelengineering.com/dir/Technologies/Hydrogen%20Detection/Hydrogen.htm
 
to determine percentage is probably tricky. We use Oneida N.Y.C. As far as 
I remember, they can determine %age by anticipate bal > H2.  
I'm not a chemical guy myself.


 
On 17 March 2011 09:09, Douglas Pauls <[log in to unmask]> wrote:
Good morning all,

I am posting this question for a colleague (not Hillman).

Take a look at this picture which Steve has graciously posted on his web
page.

http://stevezeva.homestead.com/Bowed_Electrolytic.jpg

This is an electrolytic capacitor and I don't have any access to the
processing history.  Presumably it went through reflow.  My colleague
would like to determine if there is hydrogen in this swelled device and if
so, what percentage.  There is presumably both liquid and gas inside the
swelled area which would complicate any standard residual gas analysis.
Hydrogen is too light for GCMS detection.

OK all you chemists, how would hydrogen presence and concentration be
determined here? And do you know of any commercial labs which would
perform that service?

Doug Pauls
Rockwell Collins

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site 
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2