TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wuJEB-000Bl2C; Fri, 1 Aug 97 10:02 CDT
Old-Return-Path:
Date:
Fri, 1 Aug 97 8:19:40 PDT
Precedence:
list
Resent-From:
Message-ID:
X-Mailing-List:
<[log in to unmask]> archive/latest/14468
>From willli Fri Aug 1 10:
04:31 1997
TO:
Return-Path:
<TechNet-request>
X-Loop:
X-Priority:
3 (Normal)
X-Incognito-Format:
VERSION=2.01 ENCRYPTED=NO
Resent-Message-ID:
<"knIGs.0.HwD.QgVup"@ipc>
Subject:
From:
X-Incognito-SN:
472
Cc:
Resent-Sender:
TechNet-request [log in to unmask]
From [log in to unmask] Fri Aug 8 13:
59:47 1997
Parts/Attachments:
text/plain (47 lines)
I can think of three processes that have been successful for us:

     1)  Cu/Ni/Au on circuit board, silver filled epoxy for die mount.
     2)  Thickfilm Au and Ag connection on hybrid microcircuit.
     3)  My wife's wedding ring.

I'm sure there are other processes.  Can your source point you (or me) to any 
supporting documentation?

Glenn Pelkey
Quality/Reliability Engineer
Maxtek Components Corp.


"Murphy Steve (UO/ESS)" <[log in to unmask]> Wrote:
| 
| I have been told that gold and silver are incompatible 
| materials forbonding together, and that, therefore, gold 
| finishes and silver-filled,electrically conductive 
| adhesives will not work well together.  Doesanyone have 
| any data to corroborate or contradict this 
| information?Steve 
| Murphy****************************************************
| ************************ TechNet mail list is provided as 
| a service by IPC using SmartList v3.05 
| **********************************************************
| ******************* To subscribe/unsubscribe send a 
| message <to: [log in to unmask]>   ** with <subject: 
| subscribe/unsubscribe> and no text in the body.          
| **********************************************************
| ******************* If you are having a problem with the 
| IPC TechNet forum please contact   ** Dmitriy Sklyar at 
| 847-509-9700 ext. 311 or email at [log in to unmask]      
| **********************************************************
| ******************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2