You should strive for a level of less than 100ppm oxygen, but it depends
on your reflow oven. Not all ovens are created equally. If your oven was
truly designed to be a nitro oven, it should be able to maintain this
level within the reflow chamber. It is important that you measure the
oxygen level right at the point in the oven that reflow takes place. If
your oven does not or cannot get to 75-100ppm efficiently without your
going through millions of gallons of N, don't bother. The cost of the
nitrogen use is going to be far higher than the cost of touching up 2
more DPMO. Achieving 100ppm does not mean you will reap immense
reductions in solder defects; getting your suppliers to provide
solderable parts and managing the shelf life of those parts is a much
more beneficial pursuit. Focus your efforts on that.
I have seen factory operations where the oven's best performance was
around 300-400ppm oxygen, but they had 5-6 sigma yields, and the few
defects they had were usually tied to "incidents" rather than general
solder-type defects.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Monday, May 21, 2007 3:21 PM
To: [log in to unmask]
Subject: [TN] Recommended Nitrogen Levels for Lead-free Reflow
Everyone,
I'd be interested to know what you recommend for nitrogen usage in a
lead- free reflow process utilizing fine pitch QFPs.
I've seen documentation where users were maintaining oxygen levels
everywhere from 25 to 2500 PPM. I find that range to be quite wide.
What's your experience?
Thanks in advance,
Leland
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|