Juan T. Marugán a écrit :
>Hello teachers,
>
>we have the following problem in some class 3 units: we have detected a
>white stuff inside the contacts of female connectors. It could be the main
>cause of the failures found during testing. Our thought is this substance
>could be due to a reaction between the rosin flux used when soldered the
>connectors whit the cleaning solvent (IPA)
>
>Two questions:
>
>1) Could you recommend a solvent to remove these residues. We have tried
>with 141-b, but it could damage some parts of the unit.
>
>2) We would like to send a contaminated connector to a lab for analisys.
>Could you recommend a technique to determine these substances?
>
>Thank you for your help.
>
>Juan T. Marugán
>Indra Sistemas SA
>España
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>
>
Juan,
In such a case, I would recommend to make a FT-IR analysis. This
analysis is even more efficient when made in comparison with other
substances.
We have an internal lab which does this kind of analysis for years.
Best regards,
Arnaud Grivon
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|