TECHNET Archives

March 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 27 Mar 2007 10:00:57 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Edward Mines <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; charset=iso-8859-1
From:
Edward Mines <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
My e-mail to the author of the recent inquiry about "weather coatings" did not go through.
   
  Conformal coatings protect PC boards from atmospheric moisture and hostile chemical environments but are not waterproofing.  
   
  Boards coated as directed in MIL-I-46058 and now IPC-CC-830 frequently have incomplete coverage prone to fail when in contact with liquid water.
   
  Some engineers recognize this and apply thicker coating then is recommended in the aforementioned documents and by some manufacturers. Some coatings will not cure properly in overly thick cross sections. 
   
  Encapsulation can provide the thicker layer necessary to provide complete coverage.
   
  When I was in the conformal coatings industry I helped several customers protect boards against rain and liquid sea water. Mr. Eckert, contact me off list for  details.
   
  Edward Mines
   
   

 
---------------------------------
Sucker-punch spam with award-winning protection.
 Try the free Yahoo! Mail Beta.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2