TechNetter,

Does anybody know who supply gold plating solution for deep tank ? I am
going to change the chemical because the plating efficiency is too low that
caused some trouble. Please pass information  or contact with me directly
via email if you have any good resource. I am very appreciated for your
input.

Howard Lin
Sr. R&D  Manager
Maxedge Electronic Corp.(MEC)
[log in to unmask]
FAX:886-3-4770127
TEL:886-3-4770123 Ext. 5100