Would you care to comment on some specifics as to what you consider
too high a pressure, and too fast a heat up rate?
Also what would be the dimstab consequences (assume other properties
are OK) of slightly undercuring the resin system in the press (with no post
bake)? I know that such a panel can shrink a few hundred ppm if it sees
heat later on above Tg, which can be a nuisance. I've never really known
if the dimstab coming out of the press is actually worse, but it doesn't
seem to be.
Jonathan Whitcomb IBM Endicott 607-757-1326 [log in to unmask]
Dept T49G bldg 257-2 1701 North St. Endicott NY 13760 aisle H office
X013 pager 2930 fax 607-757-1156
Geoff Layhe <[log in to unmask]>@IPC.ORG> on 10/29/2002 08:05:59 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Geoff Layhe <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: Re: [TN] Dimensional stability
If you want to improve registration between layers you need to start way
sooner than the press.
Here are a few quick pointers to improving registration/stability.
Choose cores and pre-pregs carefully. Cores with a high glass to resin
ratio
will be better for stability.
Some pre-pregs give better results than others. I've always found 2116
better than 2125 for instance.
If you use compensation factors on inner layer artwork make sure they
reflect what the laminate is doing. (Signal layers will need more
compensation than ground layers).
Brushing can stretch inners. Chemical clean is better.
Always have copper around tooling holes in inner cores.
Make sure the heat up rate in the press is not too fast. If it's too fast
it
will give too much flow and "stretch" the inner cores.
Make sure the pressure is not too high use a vacuum press if possible.
Make sure the cure time is long enough to fully cure the resin.
Cool down rate should be the same as the heat up rate. (This affects bow &
twist more than stability.
Hope this helps
Geoff Layhe
Lamar UK Ltd
-----Original Message-----
From: [log in to unmask]
[mailto:[log in to unmask]]
Sent: 29 October 2002 09:34
To: [log in to unmask]
Subject: [TN] Dimensional stability
Fellow Technetters,
Pls suggest a way out of this problem
1. If I want to reduce the dimensional instability after Multilayer
pressing, what all the variables I should consider
2. By reducing the rate of cool down, will I be able to achieve the
required stability
Thanx in advance.
Warm regards,
Madhu
**********************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the mail system admin at AT&S India Limited [log in to unmask]
This footnote also confirms that this email message has been swept by
MIMEsweeper for the presence of computer viruses.
www.mimesweeper.com
**********************************************************************
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
Private & Confidential:
This e-mail message is confidential and is intended solely for the person
or
organisation to whom it is addressed. If the message is received by anyone
other than the addressee please return the message to the sender by
replying
to it and then delete the message from your computer.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|