TECHNET Archives

October 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jason Zhao <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jason Zhao <[log in to unmask]>
Date:
Thu, 29 Oct 2009 08:50:57 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (96 lines)
Interesting.  I always think gold is the functional layer and the nickel is
there to prevent the copper migration to gold layers. 

Regards,
 
Jason Zhao
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Thursday, October 29, 2009 7:13 AM
To: [log in to unmask]
Subject: Re: [TN] Al wire bonding

Anat,

One can bond to the nickel [without the gold]!! This become especially easy
with heavier wire sizes [>2 mil].

Typically, one uses an ENIG plating.  The immersion gold results in a gold
flash of ~2-5µinches
The gold is merely there to protect the nickel from oxidizing too much.  One
actually bonds 'through' the gold layer to get to the underlying nickel.

If given a choice, I like pure soft gold instead of a hardened gold.  If you
use ENIG, you may not get much choice in your gold.

It is my opinion that the thermal history & chronology of the board has more
of an inpact on wire bond reliability than simple plating.  Eg - if one were
to reflow the board, [maybe] clean it, then let it set in que for multiple
weeks in a shop environment - I virtually guarantee you that you will note
differences in bonding characteristics as compared to a virgin board.

ENIG, or gold flash, is my answer.  Keep them moving - don't let them set
around, is my recommendation.

Steve Creswick





On Thu, Oct 29, 2009 at 3:38 AM, Anat Douek <[log in to unmask]> wrote:

>
>
> Hi,
> What is the min gold thickness required for reliable aluminum wire bonding
> ?
> Which gold type is prefered for this process?
> It is needed  for a military application.
>
> Regards,
> Anat Douek
> Process Engineer
> Herley General Microwave Israel
> tel. 972-25689455
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional information,
or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2