Kelly,
I would agree. If the solder has in fact melted onto the gold, as in Figure 10-3, it is a defect. I would err on the side of caution and venture to guess that the actual width of the gold finger is 1 mm and would apply the 10x criteria at a minimum. The 20x case can also be made depending on what is being inspected. If someone was insisting on using 4x, I would turn down the illumination and the gold vs solder color contrast would become more obvious to them.
The critical contact area is extremely pertinent to the situation.
The bigger question is why solder spheres are being left in the critical area and then being allowed to reflow. Out of control printer wipe cycles, dirty stencils, improper misprint cleaning all come to mind.
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kelly Morris
Sent: Thursday, April 21, 2011 10:21 AM
To: [log in to unmask]
Subject: Re: [TN] IPC-A-610, Solder on gold fingers - Inspection/Acceptability
I failed to clarify in my previous posting that the solder is being found in the critical contact area of the gold finger.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|