I believe Hitachi makes a halogen-free no-flow prepreg.
I also understand that standard FR-4 no-flow prepregs *will* meet the RoHS
requirements at least for now.
I.e. they don't have to be halogen free, they just can't contain
polybrominated biphenyls (PBB) or polybrominated diphenyl ether (PBDE) -
they *can* contain the ordinary bromine-containing flame retardant in FR-4
which is tetrabromo-bisphenol A (TBBPA) - and of course they can't contain
lead, mercury or cadmium.
Regards,
Tim Reeves
Process Engineer
Tyco Electronics | Printed Circuit Group | Dallas Division
503.623.1000 Ext.1120
-----Original Message-----
From: Pete menuez [mailto:[log in to unmask]]
Sent: Thursday, December 02, 2004 5:08 PM
Subject: Re: Rigid Flex Materials
I don't know if it will meet the standards but you might want to contact
Polyclad (Cookson) They were developing some new low/no flow prepregs.
pete
>From: Steve Kelly <>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>, Steve Kelly
><[log in to unmask]>
>To: [log in to unmask]
>Subject: [TN] Rigid Flex Materials
>Date: Thu, 2 Dec 2004 14:49:59 -0500
>
>Good Afternoon,
>
>Do any suppliers or fabricators know of a no-flow pre-preg which will meet
>the new European ROHS requirements. Regards Steve Kelly
>
>
>
>PFC Flexible Circuits Limited
>
>Ph: (416) 750-8433
>
>Fax: (416) 750-0016
>
>Cell: (416) 577-8433
>
>E-Mail: [log in to unmask]
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|