TECHNET Archives

June 2014

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Wayne Thayer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Date:
Mon, 23 Jun 2014 14:39:28 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (103 lines)
So the risk is:

Somehow a roll of solder, which is on the static mat with only the spool
touching it, but with some of the solder sticking out (not drooping to the
mat gets a charge on it (triboelectric due to dragging the spool as Mr.
Stadem points out, or some other way; we'll have to experiment with all the
ways this could be done inadvertently).  Then the circuit we're trying to
protect is brought close enough to the wire of solder sticking out to
discharge the solder through the static-sensitive device.  And this has to
be done without the operator touching the solder (easy if the operator wears
insulated gloves) and without the solder first touching a grounded soldering
iron.

Sounds plausible.  It would be fun to set up a controlled experiment to see
if this would be like the 20 minute gap in the Nixon tapes (I think her name
was Rosemary Woods?).  Then again, I never thought it would be possible to
start a fire while fueling your car by sliding your butt across the car seat
and then touching the handle of the filling nozzle (actually caught on
security video tapes!).

On the other hand, there may be better investments available to provide
higher reliability circuits than focusing on the dangers lurking in your
spool of solder.

Wayne

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, June 23, 2014 10:08 AM
To: [log in to unmask]
Subject: Re: [TN] ESD and solder rolls

There is if the roll of solder is anywhere on the ESD mat and is not being
handled by the operator.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: Monday, June 23, 2014 7:44 AM
To: [log in to unmask]
Subject: Re: [TN] ESD and solder rolls

Ed,

I would say that there is no ESD risk with these plastic spools in normal
use.
When solder is being used off of a spool, typically it is being fed by hand
by the operator. Since the operator is grounded, there is no risk to the
hardware.

Ben

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski
Sent: Friday, June 13, 2014 4:24 PM
To: [log in to unmask]
Subject: EXTERNAL: [TN] ESD and solder rolls

Greetings again fellow 'netters,

An operator brought up a very interesting question. The rolls upon which
wire solder is spooled are not typically "ESD safe" plastic. Is there an ESD
risk and if so, how can it be mitigated.

My immediate answer was "great question, and in all the years of being in
this business, no one that I know of has ever asked it. For the moment,
precedence has been set, so carry on, however, I will seek counsel from my
most esteemed colleagues at IPC (technet)"

Please share your wisdom, oh enlightened ones!

Ed Popielarski
Engineering Manager

[cid:[log in to unmask]]
                               970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0695
                              Cl: 949-581-6601

       "It's one kind of victory to slay a beast, move a mountain, and cross
a chasm, but it's another kind altogether to realize that the beast, the
mountain, and the chasm were of your own design."
https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.0
11188,0.033023&ctz=420&t=m&z=16&iwloc=A


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

ATOM RSS1 RSS2