Cracks propagate . . . this is not a good thing.
Guy Ramsey
American Competitiveness Institute
Senior Lab Technician / Instructor
610 362-1200 ext 107
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bissonnette,
Jean-Francois
Sent: Tuesday, February 27, 2001 10:57 AM
To: [log in to unmask]
Subject: [TN] Fractured solder joint on component side
Hi Technetters,
It is stated in IPC-A-610C that a fractured joint is considered defect in
all classes. Can anyone
confirm that it would be the same if the fracture is on the component
side? And why should
it be considered as defect if the joint on the secondary side is good.
Would the fracture
extend from the primary side to the secondary side?
Thanks in advance...
JF
WABTEC CORPORATION CONFIDENTIALITY NOTE
The content contained in this e-mail transmission is legally privileged
and confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly prohibited.
|
|
|