Polyimide is a complete resin/curing agent system and is a C stage resin
meaning it is full cured. Polyamides are a curing agents for epoxies. They
are described on page 61 as preponderantly amines according to the book
Epoxy Resin by Irving Skeist (1958)
Wrom: YUCDDJBLVLMHAALPTCXLYRWTQTIPWIGYO
To: <[log in to unmask]>
Sent: Wednesday, March 13, 2002 6:29 PM
Subject: Re: [TN] High Rel BGA Guidelines
> Bob,
>
> What's the difference between polyimide and polyamide?
>
> David A. Douthit
> Manager
> LoCan LLC
>
> "Crain, Bob" wrote:
>
> > We may soon be adding BGAs to our approved parts list for some programs.
We
> > use polyamide boards and require electrical test under vibration and
thermal
> > cycling. What are the most important factors to address to maximize our
> > success?
> >
>
> --------------------------------------------------------------------------
-------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> > To unsubscribe, send a message to [log in to unmask] with following text
in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> > To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> > Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>
> --------------------------------------------------------------------------
-------
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|