TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Leadfree Electronics Assembly Forum <[log in to unmask]>
Date:
Tue, 22 Nov 2005 11:13:27 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Phil Nutting <[log in to unmask]>
Parts/Attachments:
text/plain (35 lines)
OK, here is today's $64 question.
 
We have a vendor stating his parts are as follows;
 
(RoHS Compliant, with exemptions: 

The supplied product does contain relevant substance exempt under the
following criteria:

Lead (Pb) in high melting temperature type solders (i.e.) tin-lead
solder alloys containing more than 85% lead.)

If we have some of these parts and solder them into circuit boards in
our lead-free wave solder system, aren't we going to contaminate our
solder pot with lead?

Are these vendors off base by supplying components with "high temp"
solder to get around the RoHS requirements?  In my opinion they are
taking the easy way out for them with no concern for their customers.
 
Has anybody else encountered this and what was your solution?  I feel a
vendor change coming on.
 
Phil

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2