TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Tue, 18 Aug 1998 09:19:50 +1000
Content-Type:
text/plain
Reply-To:
"\"TechNet E-Mail Forum.\" <[log in to unmask]>, Paul Klasek" <[log in to unmask]>
Parts/Attachments:
text/plain (134 lines)
Killed the cat too , Ed
Most components , as you said, would not live with another 20'C .
Especially with LED's its a battle to keep them alive .
Would be high price and risk to pay for cheap flux and solder ; we still
foam the no clean (spray proved too messy)
Did you like that Electrovert new gas delivery (is it alpha wave ?) ?

Paul

> ----------
> From:         Ed Holton[SMTP:[log in to unmask]]
> Sent:         Tuesday, 18 August 1998 5:36
> To:   [log in to unmask]
> Subject:      Re: [TN] Hydrogen/Nitrogen saftey issues
>
> Dennis (and others) if I may ask, why do you want to put this mix in
> your
> reflow oven.  What assembly process/technolgy is this used for?  I
> asked a
> question on technet several months ago about using nitrogen/hydrogen
> in the
> reflow process, because I was told that the hydrogen, at temperatures
> above
> 300C (or 350C from another source) will actually clean the surface of
> an
> area to be soldered, thus eliminating flux.  Obviously at this
> temperature,
> you would need a high temp solder, and components that can withstand
> the
> high temperatures.  Curious minds want to know, who is using this, and
> why?
> It is my understanding that Electrovert has investigated this, but my
> contact person did not say much.  I think they are still
> investigating.
>
> CURIOUS MINDS WANT TO KNOW!!!!!!!!!!!!!
>
>
>
>
> [log in to unmask] on 08/17/98 02:39:36 PM
>
> Please respond to [log in to unmask]; Please respond to
> [log in to unmask]
>
> To:   [log in to unmask]
> cc:    (bcc: Ed Holton/Hella North America Inc.)
> Subject:  [TN] Hydrogen/Nitrogen saftey issues
>
>
>
>
> From: Dennis J Fall@TFT on 08/17/98 01:39 PM
>
>
> To:   [log in to unmask]
> cc:
> Subject:  Hydrogen/Nitrogen saftey issues
>
> I am looking for some information regarding the safety of reflow ovens
> using a 15% Hydrogen 85% Nitrogen atmosphere.  If anyone has had
> experience
> using this concentration or something close to it, please let me know.
> Maybe we can discuss any safety issues that may pertain to the
> process.
>
> Thank You,
>
> Dennis Fall                        P: 507-625-8445 x17
>
> Process Engineer                   F: 507-625-3523
>
> Thin Film Technology Corporation         mailto:[log in to unmask]
>
> 1980 Commerce Drive                http://www.thin-film.com
>
> North Mankato, MN 56003-1702
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following
>  text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section
> for additional information. For technical support contact Hugo
> Scaramuzza
> at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2