TECHNET Archives

April 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ken Bloomquist <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Bloomquist <[log in to unmask]>
Date:
Wed, 16 Apr 2008 10:03:14 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (28 lines)
No sooner do I get back and I need some help. This is an age old subject
that has once again reared its ugly head.

We have an assembly that we are building with mixed technology. We have a
kit for several thousand and we release them in work orders of 250. All of
the PWB's have the same date code 3307. We process about 500 a day.

The first 250 went through without a hitch; the second 250 had a few pin
holes in the through-hole components; the last 250 were terrible with what
I'd call severe out gassing on 50 out of 250.

What the heck would cause a drift like that from Tuesday to Wednesday?

Thank,

KennyB


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2