TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Yannick Brisson <[log in to unmask]>
Date:
Thu, 4 Nov 2004 15:42:30 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Guy <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
John Guy <[log in to unmask]>
Parts/Attachments:
text/plain (46 lines)
Yannick,
        If the holes are spaced in a regular pattern, you can break up the pad into a "Windowpane" pattern with the bars of the Windowpane covering the holes.  This should keep the solder on the top side and still give you a good joint.  If the holes are in an odd pattern, this solution may not work for you.

Hope this helps,

John G.

 -----Original Message-----
From:   TechNet [mailto:[log in to unmask]]  On Behalf Of Yannick Brisson
Sent:   Thursday, November 04, 2004 3:05 PM
To:     [log in to unmask]
Subject:        [TN] D-Pack, holes, solder

Hi everyones,

        I would like to have your input and idea on it.  we have a board
with 1 D-Pack SMT on it. For the heat sink there are some hole on the board
under the component body.  So after the oven the paste have sunk on the
other side of the board.  We don't want any solder on the other side .  We
didn't desing the board so we couldn't change it.  Do you know some trick to
block the paste from going on the back side of the board?

Thank You

Yannick

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2