That LOOKS like just a poorly cleaned decapsulation job. The stuff you're
asking about could either be from the overmold material or some deteriorating
seals in the decapsulator. So my instinct is that it's a "red herring" in your
failure analysis. This contaminant appears to be EXTREMELY thin, no more than
5 microns, because there doesn't seem to be a detectable difference in focus
height between this and adjacent circuitry (unless the image is actually a
composite of several different pictures at different focus heights).
Wayne Thayer
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, October 08, 2015 12:31 PM
To: [log in to unmask]
Subject: Re: [TN] Ropy grunge in IC
Hi Julie,
Have your photo up, it's here:
http://stevezeva.homestead.com/3CK_2nd_decap_-_multiview.jpg
Steve
On Thu, Oct 8, 2015 at 10:21 AM, Julie Silk <[log in to unmask]> wrote:
> We had an intermittent failure on a part and after decap, there was a
> rope-like line that seemed to weave in and out of the circuitry. I'm
> having Steve Gregory post a picture. I'd like your thoughts on what
> is going on. We're consulting with the supplier, but I'd like your input.
>
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary or
otherwise private information. Any unauthorized use, reproduction,
dissemination, distribution or other disclosure of the contents of this e-mail
or its attachments is strictly prohibited. If you have received this email in
error, please notify the sender immediately and delete the original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|