I agree. The nickel takes a little more time at a higher temp when using
305 to form a good IM bond. Judging from the pictures, that may not be
happening.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*
Sent: Friday, February 15, 2008 8:49 PM
To: [log in to unmask]
Subject: Re: [TN] Samsung Memory BGA Failure
Hi Phil,
How do you KNOW that "the BGA balls see 237-245 for 30 seconds minimum."
The BGA balls run significantly lower in t than anything else on your
assembly.
Given the combination of SAC+ENIG you need to run the peak reflow zone
to at least 260C.
My opinion-you just have not made any solder joints.
Werner
**************
The year's hottest artists on the red carpet at the Grammy Awards. Go to
AOL Music.
(http://music.aol.com/grammys?NCID=aolcmp00300000002565)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|