TECHNET Archives

June 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wcYSv-000BjMC; Fri, 13 Jun 97 10:40 CDT
Encoding:
28 TEXT, 24 TEXT
Old-Return-Path:
Date:
Fri, 13 Jun 97 15:55:00 GMT
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
From [log in to unmask] Tue Jun 17 11:
11:18 1997
X-Mailing-List:
<[log in to unmask]> archive/latest/13382
TO:
IPC TechNet <[log in to unmask]>
Return-Path:
<TechNet-request>
Status:
O
X-Loop:
Resent-Message-ID:
<"F75AW1.0.Q1F.udMep"@ipc>
Subject:
>From willli Fri Jun 13 10:
41:06 1997
X-MS-Attachment:
ATT04677.htm 723 06-06-1997 19:56
Message-ID:
X-Mailer:
Microsoft Mail V3.0
From:
"Dhawan, Ashok CA-WINPO2" <[log in to unmask]>
Parts/Attachments:
text/plain (65 lines)

I like the (fresh)idea. but have not seen anyone using that. May be the 
blowing air can disturb the solder while it is solidifying and leave its 
marks(footprints-duckpads). May be this can create mess of solder balls all 
around? May be this can migrate briges instead of complete removal.?Air blow 
holes /pinholes ??
Most people have sorted the solder bridging problem by matching solder mask, 
flux and wave solder parameters. Solder bridge can be due to design factors- 
vias too close to pads or lead length or lead crimping problem.
I would like to have more info on this as we also do find this problem.
ashok dhawan
[log in to unmask]
 ----------
From: Tony Stewart
To: [log in to unmask]
Subject: Hot Air Knife  after solder pot?? Anyone use this?
Date: Friday, June 06, 1997 7:45PM

I would like to retrofit a hot-air knife in our waves after wave reflow to 
reduce bridge opportunities on designs that are not optimized.
We use some Centruy 2000s and SOLTEC waves.

Tony
Eng Mgr
C-MAC Electronic Systems Inc


[[ ATT04677.htm : 2586 in ATT04677.htm ]]

<!DOCTYPE HTML PUBLIC "-//W3C//DTD W3 HTML 3.2//EN">
<HTML>
<HEAD>
<META content=text/html;charset=iso-8859-1 http-equiv=Content-Type>
<META content='"Trident 4.71.0544.0"' name=GENERATOR>

</HEAD>
<BODY>
<P><FONT face=Arial size=2>I would like to retrofit a hot-air knife in our waves 
after wave reflow to reduce bridge opportunities on designs that are not 
optimized.</FONT>

<P><FONT face=Arial size=2>We use some Centruy 2000s and SOLTEC waves.</FONT>

<P><FONT face=Arial size=2></FONT>&nbsp;

<P><FONT face=Arial size=2>Tony</FONT>

<P><FONT face=Arial size=2>Eng Mgr</FONT>

<P><FONT face=Arial size=2></FONT><FONT face=Arial size=2>C-MAC Electronic 
Systems Inc</FONT></P>

</BODY></HTML>

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2