TECHNET Archives

April 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, GRIVON Arnaud <[log in to unmask]>
Date:
Tue, 3 Apr 2012 05:46:39 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Message-ID:
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (151 lines)
Well, that's nice, Arnaud.

Sent from my Apple 2E.
Richard.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of GRIVON Arnaud
Sent: Monday, April 02, 2012 4:59 PM
To: [log in to unmask]
Subject: Re: [TN] NTC- unmeltable solder

Envoyé à partir de mon Windows phone d'Orange

----- Message d'origine -----
De: Steven Creswick <[log in to unmask]>
Env: lundi 2 avril 2012 22:29
À: [log in to unmask] <[log in to unmask]>
Objet: Re: [TN] NTC- unmeltable solder


Inge,

I prefer mine.  I make it about 80% whole wheat, 20% rye flour.

Not like that pasty white, nutritionally void stuff we get in the stores
over here.

Have a loaf in the oven now.  Makes the house smell great.

Makes fantastic grille cheese sandwiches!!


But I do cut off the crust when stuffing into water pipes.  I forget who it
was that said it, but even the slightest amount of water in the pipe will
render it unsolderable.  I have used the bread stopper trick myself.  Just
take the aerators off the faucets for a while...

Steve C

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord
Sent: Monday, April 02, 2012 3:49 PM
To: [log in to unmask]
Subject: Re: [TN] NTC- unmeltable solder

Mother's pride or what kind?
Inge

On 2 April 2012 12:38, Gerald Bogert
<[log in to unmask]>wrote:

> April 2, 2012
>
> The problem may not have anything to do with the solder used. The pipe
> could have some water remaining in it or a valve upstream of where you
> are soldering could have small leak.  Any amount of water leak can
> make it difficult if not impossible to make a solder joint.  Old
> plumbers trick by putting small piece of bread into the pipe may stop
> the leak long enough to make the solder joint.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
> Sent: Thursday, March 29, 2012 4:57 PM
> To: [log in to unmask]
> Subject: Re: [TN] NTC- unmeltable solder
>
>  Hi Blair - one other possible reason but lower on the possibility
> scale is that the solder joint, if old enough, had converted itself
> into a tin/copper joint rather than copper and solder joint. Most
> solders contain a low melting element - i.e. lead, bismuth, etc. - so
> the solder joints should go molten but if you had a high tin alloy
> with minimal lower melting point element addition, you would be trying to
"melt"
> copper/tin intermetallic which isn't going to happen.  Mike's or
> Chuck's responses are more probable explanations for what you experienced.
>
> Dave
>
>
>
> Blair Hogg <[log in to unmask]>
> Sent by: TechNet <[log in to unmask]>
> 03/29/2012 12:20 PM
> Please respond to
> TechNet E-Mail Forum <[log in to unmask]>; Please respond to
> Blair Hogg      <[log in to unmask]>
>
>
> To
> <[log in to unmask]>
> cc
>
> Subject
> [TN] NTC- unmeltable solder
>
>
>
>
>
>
> The recent discussions on rework issues reminded me of a while back
> where I needed to repair a leaky water pipe in my home. Took a chunk
> of the ceiling out, got out the plumbers torch, drained the pipes and
> started to heat. No matter what I did to the joint that was leaking I
> could not get
>
> anything to melt. Had to cut the pipe on either side of the elbow
> joint and patch in a new section. Even afer I took it out I could not
> get it apart. Not sure what happened to the solder but something
> changed it to make it unmeltable.
>
> Blair
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
> service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2