hi all
Just a question to all the BGA experts out there ;)
How would you tackle BGA assembly where there are both Pb Free BGAs and the
standard Sn/Pb BGAs on the same board?
Our paste manufacture recommended we maximise the peak as far as possible
but my concern is how would this affect the other BGAs (not Pb Free) on the
board. Would this degrade the joint due to excess heat and possibly longer
time above Eutectic for other components? What would be a good compromise
peak temperature to obtain a reliable joint?
Has anyone done something like this that could share their experience.
Thank you in advance
kind Rgds
Dennis
#################################################
***** CONFIDENTIAL *****
We apologise if this message has been sent to you in error. We are committed to protecting the confidential information of our customers, our vendors and GPC Electronics. If you have received this message in error, we would appreciate you removing it from your system and informing us of the error, so that we may continue to improve our processes.
Please note that whilst we check our outgoing mail, you should also check any attachments for viruses and defects before opening them or sending them on.
Thank you.
#################################################
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|