TECHNET Archives

April 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 14 Apr 2009 13:00:50 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Lee Whiteman <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (91 lines)
Remember, whether it's 9.8 m/sec2 or 32.2 ft/sec2, it's still 1 G.

Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Tuesday, April 14, 2009 12:03 PM
To: [log in to unmask]
Subject: Re: [TN] European Union Council Directive 80/181/EEC (Metric Directive) - NTC

Steve 
 
Your note reminded me of one the worst modifications made to the English  
system and that was the decimal inch.  This allowed  users to think they had 
a metric system equivalent and did not need to  make the change, which was a 
BIG mistake. 
 
Let go crash some more Mars explorers... ;-) 
 
Cheers, 
Joe
 
 
 
 
In a message dated 4/14/2009 8:57:29 A.M. Pacific Daylight Time,  
[log in to unmask] writes:

Mike,

As a similar aside, I have had many 'knowledgeable'  individuals verbally
refer to a 'mm' [millimeter] as a 'mil'....  ouch!

Let me assure you, that when bonding '1 mil' gold wire, I am  referring to
'0.001 inch'.  'One mil' is so much easier to say than  25.4 µm [or microns]
....[yes, I know all the arguments, but the real  problem comes in when
people do not pay attention to labels.  In the  olden days of chalk board 
and
slate, we were taught to 'mind our labels'  when it came to math.  Alas,
ignorance is bliss.]

Should anyone  have any 1 mm gold wire they wish to dispose of, I would
gladly put it into  my unemployment fund!!  I would even spring  for
shipping!!

We'll get there  eventually.

Steve

---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To  receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:  http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information,  or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------

**************Why pay full price? Check out this month's deals on the new 
AOL Shopping. (http://shopping.aol.com/?ncid=emlcntinstor00000001)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2