yes, EIT still runs it as "CITC". Current Induced Temp Cycling.
At 11:24 AM 11/23/2010, Werner Engelmaier wrote:
> Hi Louis,
>All DC current induced thermal cycling test
>methods are based on the development of this
>test methodology at Northern Telecom by Rama
>Munikoti. Since Northern Telecom had no interest
>in commercially exploiting this methodology, two
>companies developed commercially viable test
>apparatus from that original concept—PWB
>Solutions in Canada and IBM in Endicott. IBM
>may still do this internally, but the IBM test
>is commercially run by Endicut Technologies [I think this is correct].
>I hope this helps.
>Werner
>
>
>
>
>
>
>
>
>-----Original Message-----
>From: Louis Hart <[log in to unmask]>
>To: [log in to unmask]
>Sent: Tue, Nov 23, 2010 1:59 pm
>Subject: [TN] DC current induced thermal cycleing test, method 2.6.26
>
>
>TechNetters, at the end of test method 2.6.26, the document states there are
>
>'other test systems that operate on principles similar...'
>
>
>
>Please advise me of any 'other' systems you know
>of, and if you are aware of any
>
>labs that could do such testing.
>
>
>
>Thanks.
>
>
>
>Louis Hart
>
>Compunetics
>
>Monroeville, PA
>
>USA
>
>[log in to unmask]<mailto:[log in to unmask]>
>
>412-858-1272
>
>
>
>______________________________________________________________________
>
>This email has been scanned by the MessageLabs Email Security System.
>
>For more information please contact helpdesk at x2960 or [log in to unmask]
>
>______________________________________________________________________
>
>
>
>---------------------------------------------------
>
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>
>To unsubscribe, send a message to [log in to unmask] with following text in
>
>the BODY (NOT the subject field): SIGNOFF Technet
>
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>
>To receive ONE mailing per day of all the posts: send e-mail to
>
>[log in to unmask]: SET Technet Digest
>
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>
>additional information, or contact Keach Sasamori at [log in to unmask] or
>
>847-615-7100 ext.2815
>
>-----------------------------------------------------
>
>
>
>
>______________________________________________________________________
>This email has been scanned by the MessageLabs Email Security System.
>For more information please contact helpdesk at x2960 or [log in to unmask]
>______________________________________________________________________
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of
>Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts:
>send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach
>Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|