TECHNET Archives

July 2017

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Tue, 25 Jul 2017 19:42:25 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ed Popielarski <[log in to unmask]>
Message-ID:
Subject:
From:
Ed Popielarski <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Sell short!



Regards,



Ed Popielarski

Engineering Manager





                               970 NE 21st Ct.

                              Oak Harbor, Wa. 98277



                              Ph: 360-675-1322

                              Fx: 206-624-0695

                              Cl: 360-544-2289







       “It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design.”

https://goo.gl/maps/mMjg43rXeFB2





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory

Sent: Tuesday, July 25, 2017 12:00 PM

To: [log in to unmask]

Subject: Re: [TN] Sand becomintg a scarce global commodity??



Interesting topic. Didn't know that sand was becoming this scarce. I found

this:



http://pulitzercenter.org/projects/deadly-global-war-sand



Steeve



On Tue, Jul 25, 2017 at 12:52 PM, David Hillman < [log in to unmask]> wrote:



> Hi Rich - I have a number of good references sources and do track this 

> as a topic and that is the first time I have heard that silicon was an 

> issue. I suspect they may be confusing fracking sand versus other sand 

> type/applications as that is a hot topic. I would love to see their 

> reference data as it sounds quite suspicious.

>

> Dave Hillman

> Rockwell Collins

> [log in to unmask]

>

> On Tue, Jul 25, 2017 at 1:12 PM, Richard Kraszewski < 

> [log in to unmask]> wrote:

>

> > Last week I heard an interesting story  NPR  radio, claiming  that 

> > there is an upcoming global scarcity of sand.

> >

> > Seems like most  good deposits are  being mined out for concrete.  

> > This

> is

> > starting to  become a  concern for  people such as silicon wafer

> producers

> > amongst others.

> >

> >

> >

> > Anyone  hear  anything similar?

> >

> >

> > Rich  Kraszewski

> > Senior Staff Process Engineer

> > Plexus Engineering Solutions

> >

> >

> > * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *

> >

> > This e-mail and any attachments are confidential from Plexus Corp. 

> > and

> may

> > contain information which is privileged, confidential, and/or 

> > protected

> by

> > non-disclosure agreements.  They are intended solely for the use of 

> > the named addressee(s).  .  Any unauthorized use or disclosure may 

> > be unlawful.  If you are not a named addressee, you must not use, 

> > disclose, retain or reproduce all or any part of the information 

> > contained in this e-mail or any attachments If you have received 

> > this transmission in

> error,

> > please destroy it and notify us immediately by return e-mail or by

> calling +

> > 1 888 208 9005.

> >

>







--

Steve Gregory

Kimco Design and Manufacturing

Process Engineer

(208) 322-0500 Ext. -3133



-- 





This email and any attachments are only for use by the intended

recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original. 