TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"(No Name Available)" <[log in to unmask]>
Date:
Tue, 11 Aug 1998 20:21:44 EDT
Content-transfer-encoding:
7bit
Content-type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (23 lines)
Inspection criteria for 610
I think the meaning here is 1.75 power and if you see a defect but you can't
tell the exact defect then you can turn the magnification up to 4.0 power.  I
don't think it is 40 power.  The case would be for example is it a scratch on
the lead exposing basis metal or poor plating.  Turning the magnification up
to 4.0 power shows it is a scratch on the lead.  Only to identify the exact
defect is the magnification turned up.  I am not an expert so take my advise
at a limited basis.

Linda Z.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2