TECHNET Archives

June 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Genny Gibbard <[log in to unmask]>
Date:
Thu, 27 Jun 2002 08:58:16 -0600
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Genny Gibbard <[log in to unmask]>
Parts/Attachments:
text/plain (36 lines)
Maybe Michael got the answer he was looking for in response to his question
'why does it need a breakout spec' but I am confused.  I thought that what
was really being asked might have been what is the definition of 'breakout'
for an unsupported hole?  I would like to know that answer.  Is breakout the
condition where the hole may not be centred in the pad and the ring around
the hole is broken?  Is the definition any different for a plated thru hole
- possibly a break in the plating inside the hole?

Thanks,
Genny.

-----Original Message-----
From: Kathy Kuhlow [mailto:[log in to unmask]]
Sent: June 26, 2002 8:15 AM
To: [log in to unmask]
Subject: Re: [TN] Definition of Supported/ unsupported hole


In my experience a break out condition on an unsupported hole is a night
mare when you go to solder especially by hand.  The breakout causes the rest
of the pad to lift and then good luck trying to get any type of solder
joint.

Kat

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2