Rick and everyone,
Sorry I forgot one important tidbit, the microsection was good. Copper
thickness was 1.2-1.8 in the blown hole. Hence, my confusion.
Anne Ledger
> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: Tuesday, April 04, 2000 10:36 AM
> To: [log in to unmask]
> Subject: Re: [TN] Outgassing
>
> try sectioning the barrel of the hole....see what the copper thickness
> was....if the deposit in the barrel was underplated in the area where
> the
> outgassing occured...there is the culprit
>
>
> Rick Fudalewski
>
> FCT
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|