It is just another non-inspectable solder joint where the process needs
to be qualified and then tightly controlled. I have seen these used on
many products, but the process needed to be controlled or problems were
seen. If the process was controlled, they worked very well. I personally
have not seen them used for a long time, and if it were required on one
of my products today, I would attempt to perform some type of X-ray
inspection for process verification purposes.
One thing I did on a harness years ago; I changed the heat shrink tubing
to a higher temperature tubing. Then I made a tool to hold the harness
and the solder sleeve in place and shrank the tubing and reflowed the
solder sleeve all in a single pass through the reflow oven. It was
qualified, it was repeatable (automated), and it was very
cost-efficient.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Wednesday, October 26, 2005 2:44 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Sleeves
Jean-Francois,
In a former life I had used some of the heat shrinkable sleeves that
containd a band of solder. Typically I used them for soldering a drain
wire to the braid of small coax wires. It stands to reason that if not
heated fully or heated too much you could end up with a defective joint.
It will be interesting to hear what our counterparts have to say on this
topic.
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bissonnette,
Jean-Francois
Sent: Wednesday, October 26, 2005 12:30 PM
To: [log in to unmask]
Subject: [TN] Solder Sleeves
Hello Technetters,
I would like to have an expert's opinion on acceptability of solder
sleeves on harness assemblies. I have a few pictures of what I beleive
to be dubious solder flow. Help would really by appreciated.
Thanks in advance!
J-F
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|