TECHNET Archives

December 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
John Burke <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Date:
Thu, 8 Dec 2005 14:53:11 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (127 lines)
6 sigma re-ball that is what they do - they also use xrf,

I agree with Dave's concerns about the package viability at lead free temperatures,

John

John Burke
Senior Manager - Operations , Optichron
[log in to unmask]
W: 510 249 5233
M: 408 515 4992
http://www.optichron.com
Profile: https://www.linkedin.com/e/fps/2665502/

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Tremmel
Sent: Thursday, December 08, 2005 2:29 PM
To: [log in to unmask]
Subject: Re: [TN] XFS analysis

Hello,

I have a sample of standard-eutectic BGAs to reball with SAC405 solder
spheres to evaluate if, among other things, the reballed BGAs will meet RoHS
compliance.  Our customer requested XRF analysis to verify this but if ye
perveyors of the higher knowledge have better resouces than I to accomplish
this then I be at thy disposal for suggestions.

Also, if anyone has experience with lower temperature lead-free alloys, I
would be interested in recommendations on that as well.


Thank you in advance Technet,

David

>From: "Gervascio, Thomas" <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>,              "Gervascio,
>Thomas" <[log in to unmask]>
>To: [log in to unmask]
>Subject: Re: [TN] XFS analysis
>Date: Thu, 8 Dec 2005 17:05:52 -0500
>
>Is this like X Ray Fluorescence? In the case of XRF, if the solder
>thickness is too thick, then the X ray from the underlying metalization
>would be absorbed and not detected. I think about 1 to 2 mils would
>probably be the limit but dependent upon the unit. A solder ball though
>would probably be too thick to get anything other than the solder alloy
>composition.
>
>Trace Labs is a good candidate. In the southeast US, Constellation Labs
>(Largo FL- Constellation Technology Corporation 7887 Bryan Dairy Road,
>Suite 100 Largo, FL 33777)
>
>Tom
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of David Tremmel
>Sent: Thursday, December 08, 2005 1:35 PM
>To: [log in to unmask]
>Subject: [TN] XFS analysis
>
>Technet,
>
>I have 20 BGAs which our client would like XFS analysis performed.
>
>Could someone point me in the general direction of a company in the US who
>could perform this work?
>
>Thank you in advance,
>
>David
>
>_________________________________________________________________
>Consigue aquí las mejores y mas recientes ofertas de trabajo EE.UU.
>http://latino.msn.com/empleos
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>unsubscribe, send a message to [log in to unmask] with following text in the
>BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
>NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
>e-mail to [log in to unmask]: SET Technet Digest Search the archives of
>previous posts at: http://listserv.ipc.org/archives Please visit IPC web
>site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------

_________________________________________________________________
MSN Latino: el sitio MSN para los hispanos en EE.UU. http://latino.msn.com/

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2