TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Carano,Michael" <[log in to unmask]>
Date:
Thu, 10 Feb 2000 16:21:25 -0500
MIME-Version:
1.0
X-To:
Darrel Therriault <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Carano,Michael" <[log in to unmask]>
Parts/Attachments:
text/plain (149 lines)
Dear Darrel,

You mention IWT as a potential replacement for OSP. What issues are you
having with OSP that are causing you to look elsewhere? Or, are you just
looking at a second source/

Thanks,

Mike

        -----Original Message-----
        From:   Darrel Therriault [SMTP:[log in to unmask]]
        Sent:   Thursday, February 10, 2000 3:16 PM
        To:     [log in to unmask]
        Subject:        Re: [TN] White Tin PWB

        Carey,

        I'm curious......are you taking issue with the naming of the process
or the
        process itself??

        If you think IWT is not a good finish process, please elaborate.  I
am in
        the process of qualifying
        it as a potential replacement for OSP and would like to get all the
        data/opinion I can.

        Regards..........DT




        At 09:34 AM 2/10/00 -0800, you wrote:
        >Every time I see "White Tin" as a process, I get queezy.
        >
        >For the record, white tin is a metallurgical form of tin.  The
company (I'll
        >not name) that is trying to capitalize on using it as a process
name has
        >bastardized terminology.  Of course, your other choice is gray tin
which is
        >unstable with poor properties and forms at low temperatures.  So
all of you
        >are using white tin, whether you know it or not.  Otherwise, you'd
be out of
        >business.
        >
        >I'm sorry...  I just had to get it off my back.
        >
        >Carey
        >
        >-----Original Message-----
        >From: Jorge A Rodriguez <[log in to unmask]>
        >To: [log in to unmask] <[log in to unmask]>
        >Date: Thursday, February 10, 2000 8:07 AM
        >Subject: [TN] White Tin PWB
        >
        >
        > >We are about to start using immersion tin PWBs (white tin) ,  the
boards we
        > >currently use are HASL and OSP. Are there any changes with the
SMT process,
        > >component termination finish or reflow process when white tin
boards are
        >used. I
        > >know that white tin provides a better pad finish than HASL,
similar to OSP,
        >but
        > >wihout the organic coating.  Any comments.
        > >
        > >
        > >Any iformation would be appreciated.
        > >
        > >
        > >Jorge Rodriguez
        > >Process Engineer
        > >Conexant Systems Inc
        > >
        > >##############################################################
        > >TechNet Mail List provided as a free service by IPC using
LISTSERV 1.8c
        > >##############################################################
        > >To subscribe/unsubscribe, send a message to [log in to unmask] with
following
        >text in
        > >the body:
        > >To subscribe:   SUBSCRIBE TECHNET <your full name>
        > >To unsubscribe:   SIGNOFF TECHNET
        > >##############################################################
        > >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
        >additional
        > >information.
        > >If you need assistance - contact Gayatri Sardeshpande at
[log in to unmask] or
        > >847-509-9700 ext.5365
        > >##############################################################
        > >
        >
        >##############################################################
        >TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
        >##############################################################
        >To subscribe/unsubscribe, send a message to [log in to unmask] with
        >following text in
        >the body:
        >To subscribe:   SUBSCRIBE TECHNET <your full name>
        >To unsubscribe:   SIGNOFF TECHNET
        >##############################################################
        >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        >information.
        >If you need assistance - contact Gayatri Sardeshpande at
[log in to unmask] or
        >847-509-9700 ext.5365
        >##############################################################

        ##############################################################
        TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
        ##############################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
        the body:
        To subscribe:   SUBSCRIBE TECHNET <your full name>
        To unsubscribe:   SIGNOFF TECHNET
        ##############################################################
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information.
        If you need assistance - contact Gayatri Sardeshpande at
[log in to unmask] or
        847-509-9700 ext.5365
        ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2