TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier /* <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 16 Jan 2008 14:29:54 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (32 lines)
Hi Inge,
As usual people are well advised not to argue with a (this) Swede; 1) he 
usually knows what he is talking about, and 2) if not, he will drink you under the 
table.
The IMCs formed by Sn/Pb, and Sn/Ag as well, are platellet-shaped crystals 
(in cross-section they may look like needles but are always plateletts), and I 
have seen no evidence that they are solderable. Solderability simply depends on 
how much Sn, or SnPb, to which you wet, is present. So the amount of these 
IMCs affect both solderability as well as Au/Ag-embrittlement.
Inge, how is Gerd? I sure have not heard anything about him for some time.



Werner



**************
Start the year off right.  Easy ways to stay in shape.
     
http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2