hi,
i can't believe how helpful this listserv is.
you all might be interested in a tool our test people use as a last resort to find shorts. it's an infrared camera, and it requires liquid nitrogen to cool off the ir tube. basically, low current is run through the short. the ir camera picks up the short in real time as it heats up the board. it dispays the image on a crt. the current levels are controlled so that no damage is done to the board. it's paid for itself many times over.
phil
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Tuesday, April 10, 2001 12:12 PM
To: [log in to unmask]
Subject: [TN] Caps shorting on bottomside after wave...
Hi all!
This is a weird one for me. We've got some boards that have 1210 .1uf
capacitors epoxied on the bottom and are waved. Test is now telling me that
there are capacitors shorted on the bottom...they can't tell me which one (or
ones) because they are all in parallel in the circuit, and they can't tell
which one it is. So what test does is give the boards back to the operators
and have them take all the caps off (over 100) and hand solder them back on
the boards...then the board will pass test.
I stencil the glue down (I use loctite 368), the glue apertures in the
stencil more or less creates a dam of glue bewteen each pad. See the picture
at:
http://www.xdrive.com/share/986929035134m7P20WC5Rnno6fT1pb7n
I don't see how in the world a cap would short given the way the glue is
printed. I have not been able to physically see a short, nor has one been
shown to me. Test is just telling me there is a short, and when all the caps
get removed and then resoldered back down the board works...
Has anybody else ever had this weird problem? This just started here
recently...
Thanks!
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|