How thick was the Gold on these boards? We have some boards with soldering
problems in house which on surface pads have 10-15 micro-inches of
gold.There was also seen balls microscopic
balls of gold lining the top of PTHs.
-----Original Message-----
From: d. terstegge [mailto:[log in to unmask]]
Sent: Wednesday, June 21, 2000 4:41 AM
To: [log in to unmask]
Subject: Re: [TN] Ag on Ni - effect of baking
Hi Richard,
I recently had some solderability problems with Ni/Au boards, where the
boardsuppliers told us we had the problems because of baking or because of a
few days storage time between subsequent soldering steps.
But never could they show me any supporting evidence for baking being such a
bad thing for this type of board. From some helpfull Technetters (people who
I consider much more knowledgable than the average fabs-salesman dealing
with a complaint) I learned that if a Ni/Au board solders badly because of
baking, there is definitely a problem with the board.
Kind Regards,
Daan Terstegge
SMT Centre
Signaal Communications
Unclassified mail
Personal Website: http://surf.to/smtinfo
>>> Richard Tilbrook <[log in to unmask]> 06/21 9:29 am >>>
NEW MESSAGE:
Hi folks,
Sorry, I wasn't feeling well yesterday and did not explan myself at all -
the
reason I asked about baking is that we reflowed one side of a surface mount
board
(gold on nickel); we then stored it in a 45'C oven as we were expecting the
remaining parts to arrive for this very urgent job. They unexpectedly took a
week.
They even more unexpectedly didn't want to reflow properly when we tried
reflowing.
I suggested "passivation" as something for the person who brought me the
problem to
think about, though I must confess that being an industrial placement
student, I am
not best equiped to make that kind of judgement. As I try to follow many of
your TN
discussions, and occasionally add when I feel able, I was sure you'd be able
to
give better reasons as to the cause and suggestions for either prevention or
cure.
Thanks and Regards,
Richard Tilbrook
PREVIOUS MESSAGE:
Hi technetters,
I'm hoping to find out a bit more about the effect of baking (at 45 deg. C)
on
boards with gold on nickel.
I would be grateful for any info on the sibject, including times,
temperatures and
effects, such as passivation.
Thanks,
Richard TIlbrook
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|