I have seen some types AOI-equipment for inspection of PCB´s.
None of the type used any kind of chemicals to prepare the prepreg.
Instead the systems used a combination of reflective and diffuse light (key point in AOI),
which can illuminate the PCB in a way so that the prepreg looks like it were fluorescent.
I have never seen a system, which were based on fluorescence of the prepreg?
We are using the AOI-systems from Orbotech and very satisfied with the performance.
Compared to other systems it has a high ratio of reproducibility.
Best regards
Jan Thuesen
-----Oprindelig meddelelse-----
Fra: Kuwako, Fujio(MMS) [SMTP:[log in to unmask]]
Sendt: 11. juli 1997 08.36
Til: [log in to unmask]
Emne: Fw: Chemicals for AOI
Is anybody in this industry tell me what type of chemicals are being used
for giving fluorescence to the prepreg material for AOI equipment?
Kuwako
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************