TECHNET Archives

February 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Phillip Bavaro <[log in to unmask]>
Date:
Wed, 16 Feb 2011 18:21:51 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (58 lines)
For me, the short answer is don't! I'm sure the subject has been touched 
upon many times already. As Mike says, all you are doing is diluting the 
active components in the alcohol and letting them dry on again exactly 
in the places where you want them least.

However, I disagree with Mike on one point and that is that RMA flux did 
have to be cleaned off with specific solvents according to the 28 809 
standards for military purposes. It was not permitted to use it as a no 
clean flux. That having been said, many people did use it as a no clean 
flux for non-military applications, with varying degrees of success. 
Despite what many people think, these fluxes did contain halide 
activators, although the quantity was limited.

In my opinion, if you need the utmost in reliability, you should do a 
proper clean with RMA fluxes or use a suitably qualified no clean flux, 
which will give you the reliability that you desire.

Brian

On 16/02/2011 17:17, Phillip Bavaro wrote:
> What happens when the RMA liquid flux used to hand solder thru hole components
> is cleaned using an IPA bath and a brush?  Most comnponents come out bright and
> shiny but happens underneath the bodies?  Ionic testing doesn't pick up
> anything.  Thanks in advance.
>
> Phil
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2