TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 18 May 2006 14:49:11 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
"Douglas O. Pauls" <[log in to unmask]>
In-Reply-To:
MIME-Version:
1.0
Parts/Attachments:
text/plain (73 lines)
Bioact SC-10 and Kyzen Ionox series.  Both very good.

Doug Pauls




             Genny Gibbard
             <Genny.Gibbard@VC
             OM.COM>                                                    To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             05/18/2006 12:59          [TN] Board wash
             PM


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
               Genny Gibbard
             <Genny.Gibbard@VC
                  OM.COM>






Hello all,
Do any of you use liquid board wash for spot-cleaning hand assembly
operations?
We have a bulk liquid we have been fond of and purchasing for years, but
recently the formulation had to be changed by the manufacturer, and it
is much more "aromatic" than it used to be.  Complaint volume is
increasing...
We are looking for alternative suggestions.
We use no-clean solder and flux, but we spot-clean flux added to
assemblies during hand-soldering operations, since it may not get fully
heated and rendered inert.

Thanks as always for your time.

Genny

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2