low current density smut - number 1 - a 74F bath is in pretty good shape. why
wud 98F water have anything to do with the formation of smut?

2- just out of curiosity (wud need to see the panel) - how is the current
density on that/the panel/panels were the smut was formed? u said 35 asf -
but what did that actual rack get?

Rick Fudalewski

FCT

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2