TECHNET Archives

October 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Ernie Crump <[log in to unmask]>
Date:
Tue, 31 Oct 2000 14:59:24 -0500
Content-type:
text/plain; charset=us-ascii
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ernie Crump <[log in to unmask]>
Parts/Attachments:
text/plain (20 lines)
We have had a vendor use a silicone rubber mat on his platen while bonding a
heatsink to a polymide pwb, and we suspect that the silicone has become part of
the pwb surface on the one side, as the UR coating process has produced
fisheyes, and peelable coating, just on the one side.
We use Bioact-7R, alcohol and then di water to clean in a proper monitored pwb
washer, but the removal of silicone is very difficult.
What cleaners are recommended for removing it, without destroying components, or
leaching under the bonded heatsink?
Thank you.  Ernie Crump   Raytheon Systems Canada.
Phone 519-885-0110,     fax. 519-885-1178

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2