Whoa Chuck!
Have you looked at the edge of your reflowed solder product
lately? There is plenty of exposed copper along the edges
of those traces. Nickel/Gold is a viable etch resist though
it is prone to slivering and undercut becomes an issue.
Usually Ni/Au is chosen as the final finish and is used as
an etch resist only as an afterthought, but it works in
alkaline etchant.
I've found that, in order to avoid excessive slivers, the
nickel thickness has to be 0.0002" thick so it won't break
when undercut in etching.
Do we want to open the Pandora's Box of "exposed copper on
trace edges" discussion? How about exposed copper on trace
surfaces? I know our customers are dead set against exposed
copper when soldermask chips off the PWB during assembly,
yet these boards have exposed copper on trace edges all the
time and in greater area.
Regards,
Dave Sullivan
Rockwell Collins, Inc.
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Re: Gold as Etch Resist
Author: [log in to unmask] at ccmgw1
Date: 1/29/97 9:50 PM
So, if you use the Ni/Au as an etch resist, what protects the trace edges
corrosion? Do you plan to plate it twice or strip the gold? I think
the photo resist is cheaper.
Chuck Brummer, Acuson.
______________________________ Reply Separator _________________________________
Subject: Gold as Etch Resist
Author: [log in to unmask] at ccUnix
Date: 1/29/97 3:35 PM
Hello,
Please post information, experiences, and anecdotes, on using
electroplated gold as an etch resist. In particular how is the etch
rate controlled. How can the undercut be reduced to eliminate the
chance of slivers.
(Gold/Nickel/Copper/FR4 :The copper gets etched)
Thanks
Rich
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
Received: from by ccmgw1.cacd.rockwell.com (SMTPLINK V2.11)
; Wed, 29 Jan 97 21:50:39 cst
Return-Path: <[log in to unmask]>
Received: from stealth.cacd.rockwell.com (stealth) by mailserv with ESMTP
(1.40.112.8/16.2) id AA160706241; Wed, 29 Jan 1997 21:50:41 -0600
Received: by stealth.cacd.rockwell.com; id VAA17927; Wed, 29 Jan 1997 21:50:04 -0600
Received: from unknown(168.113.24.64) by stealth via smap (V3.1.1)
id xma017925; Wed, 29 Jan 97 21:49:58 -0600
Received: from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI)
id VAA13573; Wed, 29 Jan 1997 21:37:37 -0800
Resent-Date: Wed, 29 Jan 1997 21:37:37 -0800
Received: by ipc.org (Smail3.1.28.1 #2)
id m0vpjbd-0000ZCC; Wed, 29 Jan 97 17:39 CST
Resent-Sender: [log in to unmask]
Old-Return-Path: <[log in to unmask]>
From: [log in to unmask]
Date: Wed, 29 Jan 97 15:38:48 PST
Message-Id: <[log in to unmask]>
To: [log in to unmask]
Subject: Re: Gold as Etch Resist
Resent-Message-Id: <"XZgWG1.0.f8J.5_zxo"@ipc>
Resent-From: [log in to unmask]
X-Mailing-List: <[log in to unmask]> archive/latest/9758
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|