Hi Steve! Wow, ya never would have thought a simple picture of a very beat
up LCC would be so interesting!
Dave
Hi Dave,
happened to get old article from APL on desk 'Reflow attachment and reliability testing of ceramic chip carriers'. And another from Bell Labs. According to these, the packages were not so bad (at that time). Quoted:
'The general implications are that minor cracking occurs in the solder joints during tempcycling, but to date no adverse effects have been seen.....
...........from the study it appears that chip carriers provide a highly reliable, easily testable, and easy to assemble packaging technique....'
'...the solder joints withstood 1,000 cycles -40/+130 Centigrades and aging at as high as +175 Centigrades.........the failure rate at +80 C is projected to be negligible for fifty years....'
Myself, was involved in development of a computer, whereas each board had some 100 LLCCs, built on multiceramic and copper technology. Think I have some pics still from that interesting time about 20 years ago...
Ingemar Hernefjord
Ericsson Microwave Systems
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|