        I know it is late on Friday, but....  I need some opinions on this
subject!!


        IPC 610 addresses fractured solder on the secondary side of the board
after lead trimming.  It is a defect.  What if you have a capacitor mounted
on the primary side of the PCB and have to bend it over the edge of the
board so in its final position it is on the secondary side of the PCB.  We
are seeing some fractures which are understandable, but they are where the
solder fillet meets the lead.  (the little Hershey Kiss on the lead)  We
did a cross section to see if the fracture was affecting the solder in the
PTH.   It had no affect on it, just as we thought.  If the fillet was not
present, I don't believe we would have fractures.  So that being said,
would any of you out there consider this a rejectable defect?

        Connie M. Korth
        Quality Specialist
        Reptron Mfg. Services, Hibbing
        218.262.6902
        [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2