David D Hillman wrote:
> Hi TechNet - I am in quest of some information! Can you please give me
>
> feedback on the following:
>
> A) How many people are currently using the soldering iron
> solderability
> test found in MIL-STD-202, method 208?
>
> B) How often do you use the method (e.g weekly, monthly, once a year)?
>
> C) Do you feel the test method should be obsolete or does it still
> have
> merit?
>
> The feedback to these questions will be used by the JSTD-002A
> committee to
> answer the question of possibly including the soldering iron
> solderability
> test method in the next revision of 002 specification.
>
> Thanks for your assistance!
>
> Dave Hillman
> JSTD-002 CoChairman
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
Hi, Dave!
We still use method 208 for mechanical parts or special components whose
soldering area is soldered to wires by a soldering iron. We always try
first the dipping method if possible. But, I must say, that we changed
the recommended flux , we use our production no clean flux or our
production no clean soldering wire . In short, if the solder connection
looks bad, it is an indication that the part's finish is not suitable
for our specific process.
How many times?- It really depends on how often we get such parts.
Gaby
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|