I have seen variations between 200 and 1200 microinches by XRF.

I also know these ranges were customer driven.

Experimentally,  when the XRF read anything other than 60/40, one was
off the pad, and remeasurement was necessary.  Otherwise a specific
sample was faken at various locations on both sides the board and marked
as such on the report.  For example, Front Left Corner - Fiducial Pad,
and so on.

I'd like to know of any HASL Surface Tolerance specifications also.

[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2