TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Date:
Fri, 28 Apr 2006 12:30:23 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Jeffrey Bush <[log in to unmask]>
Parts/Attachments:
text/plain (67 lines)
We store HASL and ENIG for 3 years, while Silver and tin are 1 year.

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED 
           76 Technology Drive - POB 1890 
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 21
                    Fax - 802.257.0011
                       <http://www.vtcircuits.com/> 
                           

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Friday, April 28, 2006 9:03 AM
To: [log in to unmask]
Subject: [TN] Shelf life of circuit board plating

Good Friday Morning All,
 
This topic may have been previously discussed, but let me try to phrase
my "problem" completely so the answer can be simpler.
 
I have a board vendor (Fab house) stating that for my ENIG boards the
plating only has a 6 month shelf life if the package is opened.  Did I
miss something here?  I thought Gold doesn't tarnish.
 
If this is true, then Immersion Tin, Immersion Silver and ENIG all have
storage issues.
 
OK, so I open a sealed package and take out half of the boards in the
package.  I may not need the rest of the boards for many months.  So how
do I protect the unused boards?  Should I vacuum seal them?  Add a
desiccant?  If I add a desiccant, are there different desiccants which
might damage the boards?
 
I'm sure I'll have more questions right after I send this.
 
Phil

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2