TECHNET Archives

August 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joyce Koo <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Date:
Mon, 11 Aug 2008 08:25:25 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (232 lines)
March got huge plasma system specfically for desmear.  You can hang your pannel inside chamber .  
--------------------------
Sent using BlackBerry


----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Mon Aug 11 08:08:47 2008
Subject: Re: [TN] Plasma Surface Treatment For Conformal Coat

Steve,

Our plasma systems for cleaning before wire bonding, etc. do not have
nearly the energy that the plasma de-smear / ashing systems have.  While
I am sure that both types of systems will be very similar in operation,
one will just have to dial down on the horsepower when dealing with the
wire bond cleaning system.

Bottom line being that if you can see the contaminate - our plasma
systems won't get it off [there is just too much of it].  The
de-smear/ashing systems will!  We are only cleaning atomic layers of
surface contaminates, generally.

March is out in California so they haven't even begun to think about
waking up yet.

Low and Slow - Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, August 11, 2008 7:51 AM
To: [log in to unmask]
Subject: Re: [TN] Plasma Surface Treatment For Conformal Coat

Mornin' Inge!

Here's a book that looks pretty interesting. I haven't read it yet, only
found it after you asked if there were any books out there.

I don't know anything about plasma cleaning, so it would be nice if
there was something I could read to learn about it:

http://tinyurl.com/6g7n6c

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Monday, August 11, 2008 6:05 AM
To: [log in to unmask]
Subject: Re: [TN] Plasma Surface Treatment For Conformal Coat

Trikeman,

late reaction...I agree with Watt you say. One problem here: most of us
know too little about running these machines. Do you know about any good
books to place in the hands of our technischzans?

Inge




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Creswick, Steven
Sent: den 6 februari 2007 20:37
To: [log in to unmask]
Subject: Re: [TN] Plasma Surface Treatment For Conformal Coat

Joe,

From a microelectronics standpoint [hermetic type of stuff] I have
always been under the impression that removal of silicone residue with
standard gases such as Argon, Oxygen, Nitrogen, or Argon+Hydrogen mixes
was not reasonably possible - talking RF plasmas in a partially
evacuated chamber, here.  Our best plan, was not to have it [silicone]
there in the first place - silicones have a really nasty tendency to
migrate all over the place, on occasion.

The greatest part of my fear of placing a silicone containing part
within the chamber is that some of what gets dislodged from the piece in
question may deposit on the chamber walls [instead of getting sucked out
the vacuum].  This can mean that the next part to go into the chamber
may get a smattering of this as it becomes knocked from the chamber
walls.  This would not be good for a part which was going to be wire
bonded, for example.

At our power levels, angstoms, or atomic layers, of contaminates are
removed.  I don't normally attempt to remove visibly thick layers of
contaminates with the plasma because doing so usually either takes a
long, long, time and/or the parts become hot and/or discolored [eg O2
will turn silver black.  Go long enough and SnPb solder will get dark
and dull looking, etc.].

A 'quicky' O2 plasma - say 5 minutes, at 150W, at about 150-200 mT will
do a nice job of activating the surface of many plastics for promotion
of adhesive adhesion though.  I have little doubt that it would also
improve the wetting characteristics of your bare laminate and/or solder
mask, but I would not necessarily lay claim that it would remove gobs of
organics [within a reasonable time frame, that is].

I'm interested in hearing what Yoda Ingemar and D Hillman have to say on
the matter.

PS - Ingemar, I had -16F, outside air temp this morning [-14F
yesterday].  Getting more like your neck of the woods each day!  Have
had enough, thank-you.

Steve



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US
SSA)
Sent: Tuesday, February 06, 2007 11:23 AM
To: [log in to unmask]
Subject: [TN] Plasma Surface Treatment For Conformal Coat

While we're on the subject of CC, does anybody use plasma to remove
stubborn organic residues (e.g. silicones) from board surfaces, or
otherwise change the surface energy to promote coating adhesion?

We're not talking about long or aggressive exposure here, just enough to
remove a thin layer of contaminant, or roughen the surface of a glossy
soldermask.  So I'm not much concerned about removing markings or
anything, but are there any other potential pitfalls?

Joe Kane
BAE Systems
Johnson City, NY

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------



THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS
SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED
ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If
you are not the intended recipient, you are hereby notified that any
review, distribution, or copying of this communication is strictly
prohibited.  If you have received this communication in error, please
immediately notify the sender by return e-mail, and delete this e-mail
message and any attachments from your computer.




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
 
 
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer. [gntx v.1]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2