TECHNET Archives

1995

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipchq.com (Smail3.1.28.1 #2) id m0s546f-0000GeC; Fri, 28 Apr 95 23:26 CDT
Encoding:
33 Text
Old-Return-Path:
<gagme!ccmail.us.dell.com!Thad_McMillan>
Date:
Fri, 28 Apr 95 16:14:40 CST
Precedence:
list
X-Loop:
From [log in to unmask] Thu Apr 25 15:
24:05 1996
Resent-Sender:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/444
TO:
Return-Path:
Resent-Message-ID:
<"G-pQ52.0.rNA.Z_Rel"@ipc>
Subject:
From:
"Thad McMillan" <[log in to unmask]>
Resent-From:
Message-Id:
Parts/Attachments:
text/plain (36 lines)
     1 oz is typical, sometimes 1/2 oz for thinner boards.  For both SMT & 
     PTH.
     
     US designs are almost all English,  Japan prefers metric.  Don't know 
     about other countries.  Most board shops can handle data in either 
     format.
     
     Typical pad sizes for microvias are 25 mil for high density designs, 
     30 mils for normal.
     
     Hope this helps.
     
     Thad [log in to unmask]
     
______________________________ Reply Separator _________________________________
Subject: SURVEY
Author:  [log in to unmask] at Dell_UNIX
Date:    4/28/95 1:23 PM


IPC Folks,
    I'm taking a informal and non scientific survey for use in making 
decisions about repairs of electronic boards.  Your answers will be 
appreciated.
What weight copper is the most commonly used on PTH boards?  1 or 2 OZ. 
What weight copper is most often used on SMT boards?
Are boards built to metric or English measurements? 
What is the average size pad on pth boards?
     
Answers may be made back through the Technet or to 
[log in to unmask]                     Thanks! 